Hastelloy C-276 LEMBAR DATA MATERIAL
Deskripsi Produk
HT PIPE nyedhiyakake Hastelloy C276 Nikel alloy round bar, Alloy C276 Bar supplier ing China. 2.4819 bar babak, Alloy C276 rod, UNS N10276 rod, Alloy C276 flat Bar, Hastelloy C276 bar kothong, Hastelloy C276 Nikel alloy babak supplier bar, eksportir.
Apa karakteristik Hastelloy C276?
● resistance karat banget ing ngurangi lingkungan
● Resistance luar biasa kanggo solusi kuwat saka uyah oksidasi, kayata ferric lan cupric chloride
● Isi nikel lan molybdenum dhuwur nyediakake resistance karat apik ing lingkungan ngurangi
● Isi karbon kurang sing nyilikake udan karbida wates gandum sajrone welding kanggo njaga resistensi korosi ing zona sing kena panas saka sambungan sing dilas
● Resistance kanggo karat lokal kayata pitting lan kaku-korosi retak
● Salah siji saka sawetara bahan kanggo tahan efek korosif saka gas klorin udan, hipoklorit lan klorin dioksida
Hastelloy C276 Nikel alloy round bar Komposisi Kimia,%
Ni | Mo | Cr | Fe | W | Co | Mn | C | V | P | S | Si |
Sisa | 15.0-17.0 | 14.5-16.5 | 4.0-7.0 | 3.0-4.5 | 2,5 maks | 1.0 maks | .01 maks | .35 maks | .04 maks | .03 maks | .08 maks |
Spesifikasi
Spesifikasi ASTM
Pipa Smls | Pipa Welded | Tube Smls | Tube Welded | Lembaran / piring | bar | Forging | Fitting | Kawat |
B622 | B619 | B622 | B626 | B575 | B574 | B564 | B366 |
Hastelloy C276 Sifat Fisik
Titik lebur: 1325-1370 ℃
Kapadhetan: 8,90 g/cm3
Alloy C276 Bar Properties Mechanical
Sifat mekanik | Tarik, min, ksi[MPa] | Ngasilake, min, ksi[MPa] | Elongation, %(min) |
Hastelloy C276 | 100[690] | 41[283] | 40 |
Sifat Tensile Suhu Kamar Khas saka Material Annealed
Formulir produk | Tarik (ksi) | .2% Ngasilake (ksi) | Elongation% |
bar | 110.0 | 52.6 | 62 |
piring | 107.4 | 50.3 | 67 |
Lembaran | 115.5 | 54.6 | 60 |
Tube & Pipa | 105.4 | 45.4 | 70 |