Baja Tahan Karat Pengerasan Presipitasi

  • Lembar Data Materi 17-4PH

    Pengenal internasional

    AISI 630, ASTM A564-89 17-4PH, JIS SCS24 / SUS630, AFNOR Z7CNU15-05 / Z7CNU17-04

  • Baja Tahan Karat Pengerasan Presipitasi

    Paduan Suhu Tinggi Komposisi kimia Kelas C Si Mn SP Cr Ni Mo Cu Nb Al liyane ora luwih saka 0Cr17Ni4Cu4Nb 0.07 1 1 0.035 0.03 15.5~17.5 3~5 - 3~5 0.15~0.7 0.15 ~ 0.45 ~ 35 0.03 16~18 6.5~7.5 - ≤0.5 - 0.75~1.5 - 0Cr15Ni7Mo2Al 0.09 1 1 0.035 0.03 14~16 6.5~7.75 2~3 - - 0.75 ~ 0.75 ~ 0.75 ~ 0.035 0.03 14~15.5 3.5~...