Alloy Suhu Dhuwur

◆Nitronic50 (S20910 / XM-19) yaiku baja tahan karat austenitik sing ditingkatake nitrogen, sing utamane digunakake ing industri petrokimia, tekstil, pangolahan panganan lan laut.

◆Nitronic60 (S21800 / Alloy218) wis resistance oksidasi suhu dhuwur banget lan kinerja impact suhu kurang, lan utamané digunakake ing efektif anti-nyandhang lan ngeruk alloy bridge pins lan proyèk tombol liyane.

Komposisi kimia

sasmita

C

Si

Mn

S

P

Cr

Ni

Fe

Mo

Ti

Cu

Nb

N

liyane

ora luwih saka

Nitronik50

0.06

1

4~6

0.03

0.04

20.5~23.5

11.5~13.5

dhasar

1.5~3

-

-

0.1~0.3

0.2~0.4

-

Nitronik60

0.1

3.5~4.5

7~9

0.03

0.04

16~18

8~9

dhasar

0.08~0.18

-

Properti paduan minimal

sasmita

negara

kekuatan tarik RmN/m㎡

Kekuwatan Ngasilake Rp0,2N/m㎡

Elongasi As%

Brinell atose HB

Nitronik50

Perawatan solusi

690

380

35

-

Nitronik60

Perawatan solusi

600

320

35

-